MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Formosa Plastics Formolene® FL2202A LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Product Description: Formolene® FL2202A is a low density polyethylene offering good balance of optical properties and mechanical properties. Formolene® FL2202A is formulated with slip and antiblock for use in applications offering excellent extrusion processing and film applications offering excellent extrusion processing and film optical properties.

Availability: North America

Additive: Antiblock; Slip

Features: Good Optical Properties; Low Density

Uses: Bags; Blending; Film; Food Packaging; Laminates; Liners; Packaging; Shrink Wrap

Processing Method: Extrusion; Film Extrusion

Information provided by Formosa Plastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ASTM D1505
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.0 MPa
@Thickness 0.0381 mm
1600 psi
@Thickness 0.00150 in
Blown Film; ASTM D882
Film Tensile Strength at Yield, TD 11.0 MPa
@Thickness 0.0381 mm
1600 psi
@Thickness 0.00150 in
Blown Film; ASTM D882
Film Elongation at Break, MD 330 %
@Thickness 0.0381 mm
330 %
@Thickness 0.00150 in
Blown Film; ASTM D882
Film Elongation at Break, TD 550 %
@Thickness 0.0381 mm
550 %
@Thickness 0.00150 in
Blown Film; ASTM D882
1% Secant Modulus  207 MPa
@Thickness 0.0381 mm
30000 psi
@Thickness 0.00150 in
MD, Blown Film; ASTM D882
 228 MPa
@Thickness 0.0381 mm
33000 psi
@Thickness 0.00150 in
TD, Blown Film; ASTM D882
Elmendorf Tear Strength MD 150 g
@Thickness 0.0381 mm
150 g
@Thickness 0.00150 in
Blown Film; ASTM D1922
Elmendorf Tear Strength TD 120 g
@Thickness 0.0381 mm
120 g
@Thickness 0.00150 in
Blown Film; ASTM D1922
Dart Drop Test 80.0 g
@Thickness 0.0381 mm
0.176 lb
@Thickness 0.00150 in
Blown Film; ASTM D1709
Film Tensile Strength at Break, MD 24.8 MPa
@Thickness 0.0381 mm
3600 psi
@Thickness 0.00150 in
Blown Film; ASTM D882
Film Tensile Strength at Break, TD 22.1 MPa
@Thickness 0.0381 mm
3200 psi
@Thickness 0.00150 in
Blown Film; ASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 6.1 %
@Thickness 0.0381 mm
6.1 %
@Thickness 0.00150 in
Blown Film; ASTM D1003
Gloss 63 %
@Thickness 0.0381 mm
63 %
@Thickness 0.00150 in
45°, Blown Film; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFPCR751 / 311444

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.