MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Multibase Multi-Flex® TPE A 6821 BLK
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: This product is based on Kraton G and PP suitable for automotive applications and meets GM, Ford, and Chrysler specifications. Multi-Flex TPE contains Kraton™ G.

Data provided by Multibase.

Key Words: Thermoplastic Elastomer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ASTM D792
Linear Mold Shrinkage 0.014 cm/cm0.014 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inASTM D955
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 230 °C
10 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 686810 sec; ASTM D-2240
Tensile Strength, Ultimate >= 5.50 MPa>= 798 psiASTM D638
Elongation at Break >= 1000 %>= 1000 %ASTM D638
Flexural Modulus 0.0345 GPa5.00 ksimethod 1, Proc.B; ASTM D-790
Tear Strength 24.5 kN/m140 pliASTM D624
Compression Set  45 %
@Temperature 70.0 °C
45 %
@Temperature 158 °F
for 70 hours at 70°C; ASTM 395
 65 %
@Temperature 100 °C
65 %
@Temperature 212 °F
70 hours at 100°C; ASTM 395
 17 %
@Temperature 23.0 °C,
Time 252000 sec
17 %
@Temperature 73.4 °F,
Time 70.0 hour
ASTM 395

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel
ATI Allegheny Ludlum H13 Tool Steel, UNS T20813
Multibase Multi-Flex® TPE A 5904 LC BLK
Multibase Multi-Flex® TPE A 6821 NAT

PLA040 / 49501

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.