MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Hexcel® HexPly® M81/42%/370T2/CHS-12K Epoxy Resin Matrix
Categories: Polymer; Thermoset; Epoxy

Material Notes:

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1100 MPa160000 psiEN2561
Tensile Modulus 66.0 GPa9570 ksiEN2561
Flexural Strength 1020 MPa148000 psiEN 2562
Flexural Modulus 56.0 GPa8120 ksiEN 2562
Compressive Strength 840 MPa122000 psiEN 2850B
Shear Modulus 4.90 GPa711 ksiIn plan; ASTM D3518
Shear Strength 63.0 MPa9140 psiInterlaminar; EN 2563
 90.0 MPa13100 psiIn plan; ASTM D3518
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature -18.0 °C
12.0 Month
@Temperature -0.400 °F
 
Descriptive Properties
G1 C1000 J/m2EN 6033
 14 cm2Damage Area, ASTM D7136/D7137 - 6,6J/mm
 200 MPaStrength, ASTM D7136/D7137 - 6,6J/mm
 28 mmIndentation, ASTM D7136/D7137 - 6,6J/mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9168 / 322324

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.