MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Astralloy AstraWear 450F 450 BHN Wear Resistant Steel
Categories: Metal; Ferrous Metal; Martensitic

Material Notes: AstraWear 450F is a water tempered martensitic steel, with typical hardness of 450 BHN, which offers a real response to wear from abrasion. Its resistance, high hardness, and yield strength make it highly resistant to plastic deformation and wear from scraping and impact. AstraWear 450F shows resistance to wear typically equal to 4 times and any yield strength 3 times greater than those of a A572-50 (S355) steel. Using AstraWear 450F represents a major improvement in terms of service life and lightening of equipment by reducing thickness. AstraWear 450F is easy to process, has good welding capacity and good bendability, considering its outstanding mechanical properties. This steel is especially suited for applications in quarries, construction, mines, cement plants, and the iron and steel industry, among others. AstraWear 450F is a grade especially suited for manufacturing truck bodies.

Information provided by Astralloy, a Nucor Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 430 - 480
Tensile Strength 205 ksi
Tensile Strength, Yield 175 ksi
Elongation at Break 12 %
Charpy Impact 20.0 ft-lb
@Temperature -40.0 °C
Bend Radius, Minimum 4.0 t
@Diameter <=50.8 mm
Perpendicular to Grain Direction
 5.0 t
@Diameter <=50.8 mm
Parallel to Grain Direction
 
Component Elements PropertiesOriginal ValueComments
Boron, B <= 0.0030 %
Carbon, C <= 0.23 %
Chromium, Cr <= 1.0 %
Iron, Fe >= 95.3 %As Balance
Manganese, Mn <= 1.55 %
Molybdenum, Mo <= 0.50 %
Nickel, Ni <= 1.0 %
Phosphorus, P <= 0.025 %
Silicon, Si <= 0.40 %
Sulfur, S <= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Chromflex 12C27 Strip steel
Astralloy AstraWear 400F 400 BHN Wear Resistant Steel
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition CH 900
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition C
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 900

NNUCOR913 / 233187

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.