MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Lubri-Tech™ AT-25GB/5T-2S Acetal-Copolymer, Glass Bead Filled, PTFE/Silicone Lubricated  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes:

Description/Features:

  • Glass Bead Filled
  • PTFE/Silicone Lubricated

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.618 g/ccASTM D792
Water Absorption 0.020 %
@Thickness 3.17 mm
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0095 - 0.015 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 5500 psiType 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 3.0 %Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 340000 psiType 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 9000 psiASTM D790
Flexural Modulus 340 ksiASTM D790
Izod Impact, Notched 1.10 ft-lb/in
@Thickness 3.17 mm,
Temperature 23.0 °C
Method A, Injection Molded; ASTM D256
 
Processing PropertiesOriginal ValueComments
Melt Temperature 400 - 440 °FMolding
Mold Temperature 130 - 160 °F
Drying Temperature 160 °F
Dry Time 2 hour
 
Descriptive Properties
Product FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 901 TFE 10 Z Polysulfone (PSU), Glass Fiber - PTFE Lubricated - FDA Compliant Ingredients
Mitsubishi Chemical Advanced Materials Ketron™ GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone
LNP Lubricomp® KFL-4032 ER BK8-115 Acetal (POM) Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
Evonik Trogamid® T-GF35 35% Glass Reinforced Amorphous Nylon
Evonik Trogamid® BX9724 40% Glass Reinforced Nylon Blend

PH1PO0176 / 43411

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.