MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

(Viewing data as-entered. Click here to return)
Saint-Gobain Meldin® 3110 Thermoplastic Bearing Material
Categories: Polymer; Thermoplastic

Material Notes: 3110 has a very low coefficient of friction and is particularly well suited for use with soft mating surface materials such as aluminum and soft stainless steel. Meldin® 3100 materials have excellent mechanical properties, in tension and compression, and maintain an impressive level of these attributes as operating temperatures increase. These properties add extreme strength and rigidity to component parts, even in narrow cross-sections.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85ASTM D785
Hardness, Shore D 80ASTM D2240
Tensile Strength 54.3 MPaASTM D638
Elongation at Yield 7.5 %ASTM D638
Tensile Modulus 1.18 GPaASTM D 638
Flexural Strength 82.4 MPaASTM D790
Flexural Modulus 3.18 GPaASTM D790
Compressive Strength 100 MPaASTM D695
Compressive Modulus 1.78 GPa
@Temperature 23.0 °C
ASTM D695
Izod Impact, Notched 20.3 J/mASTM D256
Coefficient of Friction 0.20Saint-Gobain
K (wear) Factor 11.95 x 10-8 mm³/N-MASTM D3702
 
Thermal PropertiesOriginal ValueComments
CTE, linear 39.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 214 °CASTM D648
Glass Transition Temp, Tg 233 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LNP Faradex MS-1002 Polypropylene, Stainless Steel Fiber
Avient Stat-Tech™ ST5220-0004 CP4D EG Black Polypropylene Impact Copolymer (PP Impact Copolymer)

PSTGQ997 / 108552

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.