MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Copper Alloy, UNS C66200, HR02
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: 1/2 Hard and Stress Relieved

Fabrication Properties: Excellent Suitability – Capacity for Being Cold Worked, Capacity for Being Hot Formed

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 448 MPa65000 psi
Tensile Strength, Yield 414 MPa60000 psi0.2% Offset
Elongation at Break 15 %15 %
Tensile Modulus 120 GPa17400 ksi
Modulus of Rigidity 46.2 GPa6700 ksi
Poissons Ratio 0.300.30
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000490 ohm-cm0.00000490 ohm-cm35% IACS
Magnetic Permeability 0.990.99
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 12.5 W/m-K87.0 BTU-in/hr-ft²-°F
Melting Point 1027 - 1068 °C1881 - 1954 °F
Solidus 1027 °C1881 °F
Liquidus 1068 °C1954 °F
Annealing Point 249 - 599 °C480 - 1110 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 649 - 954 °C1200 - 1750 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 86.6 - 91 %86.6 - 91 %
Iron, Fe <= 0.050 %<= 0.050 %
Lead, Pb <= 0.050 %<= 0.050 %
Nickel, Ni 0.30 - 1.0 %0.30 - 1.0 %
Phosphorus, P 0.050 - 0.20 %0.050 - 0.20 %
Tin, Sn 0.20 - 0.70 %0.20 - 0.70 %
Zinc, Zn 7.1 - 12.9 %7.1 - 12.9 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC66200x2 / 292268

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.