MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Pyro-Paint™ 634-ZO High Temperature Refractory Coating, ZO >95%
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: This highly-filled zirconium oxide-based coating produces a hard, chemically-resistant protective layer which is stable with aluminum, molybdenum, platinum, rhodium, and titanium. It is ideal for sealing porous ceramics and protecting other ceramic, graphite and metal structures up to 3270 °F. Exceptional for coating resistance wire heating elements in furnaces, protecting them from residue buildup which causes arcing and reduced element life.

Key Words: Coatings
Vendors: Aremco’s Pyro-Paint refractory coatings offer the ultimate protection of high temperature graphite, metal and refractory structures used in the processing of ceramics, glasses, metals, and plastics. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.02 g/cc2.02 g/cc
Solids Content 29.6 %29.6 %volume
 59 %59 %weight
pH 11 - 1211 - 12Coating pH
Viscosity 1000 - 2000 cP1000 - 2000 cP
Thickness 25.4 microns1.00 milDry Film Thickness
 86.4 microns3.40 milWet Film Thickness
Storage Temperature 4.44 - 32.2 °C40.0 - 90.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1800 °C3270 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 10.0 - 32.2 °C50.0 - 90.0 °FApplication Temperature
Cure Time 120 min
@Temperature 93.3 °C
2.00 hour
@Temperature 200 °F
>2 Hour Air Set Required Prior to Curing
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorOff-White
Coverage ft2/gal474Theoretical Coverage at 1 mil dry film thickness
Thinner634 ZO-T
Weight/Gallon14.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CAREM65 / 606

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.