MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Westlake Elevate™ EF598 9% Ethylene Vinyl Acetate Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Westlake EF437 resin is a 2.5% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low temperature brittleness properties.
    Application/Uses:
  • High clarity packaging
  • Light and medium duty produce bags
  • Linear blend component for sealing and clarity
FDA: This material complies with FDA regulations in 21 CFR, section 177.1350. Kosher Compliant.

All information provided by Westlake Chemical

Key Words: Excellent optical and strength properties. 9% EVA.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Methyl Acrylate Content 9.0 %9.0 %
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 400 %400 %
Film Elongation at Break, TD 800 %800 %
Dart Drop 6.69 g/micron170 g/milASTM D1709
Film Tensile Strength at Break, MD 27.6 MPa4000 psiASTM D638
Film Tensile Strength at Break, TD 20.7 MPa3000 psiASTM D638
1% Secant Modulus, MD 89.6 MPa13000 psiASTM D882
1% Secant Modulus, TD 110 MPa16000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 2.7 %2.7 %ASTM D1003
Gloss 80 %80 %at 45°
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
processExtrusion
 Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eurofoam Evacell EVA 50/S EVA + NR Foam
Micropol E332 Rotational molding powder based on a random EVA copolymer
Innospec FLEXAREN® 14006 EVA-Copolymer
Innospec FLEXAREN® 07000 EVA-Copolymer
Honeywell A-C® 540 EVA copolymer

PWESF8924 / 133285

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.