MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lotte Advanced Materials Infino® FS-1030 PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes:

Information provided by Lotte Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ASTM D792
Melt Flow 12.0 g/10 min
@Load 5.00 kg,
Temperature 250 °C
12.0 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 61.8 MPa8960 psi50 mm/min; ASTM D638
Tensile Strength, Yield 63.7 MPa9250 psi50 mm/min; ASTM D638
Elongation at Break 30.0 %30.0 %50 mm/min; ASTM D638
Flexural Strength 88.3 MPa12800 psi2.8 mm/min; ASTM D790
Flexural Modulus 2.35 GPa341 ksi2.8 mm/min; ASTM D790
Izod Impact, Notched  2.45 J/cm
@Thickness 6.35 mm
4.59 ft-lb/in
@Thickness 0.250 in
ASTM D256
 7.35 J/cm
@Thickness 3.17 mm
13.8 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 113 °C235 °FB/50; ISO 306
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 2.00 mm
V-0
@Thickness 0.0787 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 5VB
@Thickness 2.00 mm
5VB
@Thickness 0.0787 in
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
Shrinkage, MD 0.00400 - 0.00700 %
@Thickness 3.20 mm
0.00400 - 0.00700 %
@Thickness 0.126 in
ASTM D955
Shrinkage, TD 0.00400 - 0.00700 %
@Thickness 3.20 mm
0.00400 - 0.00700 %
@Thickness 0.126 in
ASTM D955

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLOTT9427 / 325909

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.