MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Westlake Mxsten CV77526 Polyethylene Plastomer
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Mxsten CV Plastomer CV77526 resin is a polyethylene plastomer designed for blown film extrusion and food packaging that contains no slip and no antiblock additives. Films produced with this resin exhibit a very low seal initiation temperature with a broad hot tack window. This resin grade complies with 21 CFR 177.1520. Blown film processing temperatures of 420°F - 450°F are recommended for Westlake Chemical CV77515. Gauge of test specimens 1.0 mil fabricated on a 6" die, 2.5" 24:1 L:D barrier screw, 2.4:1 BUR, 100-mil die gap, 15" frostline height, 450°F melt temperature, and 7.5 lb/hr/inch die output. Density results are on Base Resin.

Key Words: Very low seal initiation temperature with a broad hot tack window
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccASTM-D4883
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM-D1238
 
Processing PropertiesOriginal ValueComments
Processing Temperature 420 - 450 °F
Blow-up Ratio (BUR) 2.4
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
processBlown Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals NILO® Alloy K Controlled-Expansion Alloy
Silon Tabond 3032 Adhesive Resin
REXtac Rextac® RT 2115 Amorphous Polyalphaolefin (APAO)
ICO Polymers ICORENE™ 155-1326 LMDPE Rotational Molding Resin
ICO Polymers ICORENE™ 110-1016 LMDPE Rotational Molding Resin

PWESF9010 / 106847

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.