MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Unival™ DMDB-6400 NT 7 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Product Description: Unival™ DMDB-6400 NT 7 HDPE is a multi-purpose polymer designed for producing containers used to package dairy, water and fruit drinks. In addition, it can be blow molded into other thin-walled parts and houseware items.
Main Characteristics:
  • Maximum rigidity
  • High impact strength
  • Top load strength
  • Moderate swell
  • Improved melt stability
Compiles with: US FDA 21 CFR 177.1520©2.2; EU No 10/2011

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520(c)2.2; EU No 10/2011

Form: Pellets

Processing Method: Blow Molding

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.963 g/cc0.0348 lb/in³ASTM D792
ESCR 100% Igepal® 20 hour
@Temperature 50.0 °C
20 hour
@Temperature 122 °F
F50; ASTM D1693
Melt Flow  0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 57 g/10 min
@Load 21.6 kg,
Temperature 190 °C
57 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6666ASTM D2240
Tensile Strength at Break 24.1 MPa3500 psiASTM D638
Tensile Strength, Yield 31.7 MPa4600 psiASTM D638
Elongation at Break 1000 %1000 %ASTM D638
Elongation at Yield 7.0 %7.0 %ASTM D638
Flexural Modulus 1.30 GPa188 ksi2% Secant; ASTM D790B
Tensile Impact Strength 84.0 kJ/m²40.0 ft-lb/in²Type S; ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Melting Point 133 °C271 °F
Crystallization Temperature 120 °C248 °F
Deflection Temperature at 0.46 MPa (66 psi) 76.1 °C169 °FUnannealed; ASTM D648
Vicat Softening Point 131 °C268 °FASTM D1525
Brittleness Temperature <= -76.1 °C<= -105 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF573 / 311266

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.