MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF Pluracol® 1578 Rigid Polyol
Categories: Fluid

Material Notes: Description: Pluracol® 1578 polyol is a general purpose aromatic initiator-based polyol for rigid foams for use in a variety of applications. It is attractively priced for consideration for foaming insulated panels, refrigerators, trailers, furniture, etc., by pour-in-place or frothing techniques. Foams made with Pluracol 1578 are characterized by fine cell structure, low K factor, and good dimensional stability. Pluracol 1578 is not recommended for use in quasi-prepolymer preparation.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.062 g/cc
@Temperature 70.0 °C
0.03837 lb/in³
@Temperature 158 °F
 1.069 g/cc
@Temperature 40.0 °C
0.03862 lb/in³
@Temperature 104 °F
 1.075 g/cc
@Temperature 25.0 °C
0.03884 lb/in³
@Temperature 77.0 °F
Viscosity  224 cP
@Temperature 70.0 °C
224 cP
@Temperature 158 °F
 3000 cP
@Temperature 40.0 °C
3000 cP
@Temperature 104 °F
 18600 cP
@Temperature 25.0 °C
18600 cP
@Temperature 77.0 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.050 %<= 0.050 %STI 3062
 
Descriptive Properties
ColorAmber Liquid
Hydroxyl Number380-410 mg KOH/gSTI 3007/3162

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Pluracol® 726 Specialty Polyol
BASF Pluracol® 628 Specialty Polyol
BASF Pluracol® 593 Specialty Polyol
BASF Pluracol® 3042 Specialty Polyol
BASF Pluracol® 2100 Slabstock HR Foam Polyol

PBASG0778 / 132411

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.