MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik Kanthal 50 HT Thermostatic bimetal
Categories: Metal; Superalloy; Iron Base

Material Notes: KANTHAL 50 HT is a high temperature type thermostatic bimetal which is recommended for use in corrosive environments in the temperature range -20 to +550 °C.

Typical applications for KANTHAL 50 HT are in circuit breakers, motor protection units, thermostats, shower mixers, etc.

High-expansive component: 18-10 Alloy(2333 Designation, 50% of thickness)

Low-expansive component: 17 Alloy (2320 Designation, 50% of thickness)

Information provided by Sandvik

Composition:

  • High-expansive component: Designation 2333; 18% Cr; 10% Ni; Bal. Fe
  • Low-expansive component: Designation 2320; 17% Cr; Bal. Fe
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 155High-expansive component
 180Low-expansive component
 240Low-expansive component, Cold-worked 20%
 340High-expansive component, Cold-worked 20%
Tensile Strength, Ultimate 450 MPaLow-expansive component
 730 MPaHigh-expansive component
Tensile Strength, Yield 310 MPaLow-expansive component
 370 MPaHigh-expansive component
Elongation at Break 30 %Low-expansive component
 50 %High-expansive component
Modulus of Elasticity 200 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000635 ohm-cm
@Temperature 0.000 °C
Bimetal
 0.0000780 ohm-cm
@Temperature 200 °C
Bimetal
 0.0000830 ohm-cm
@Temperature 300 °C
Bimetal
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µm/m-°C
@Temperature 30.0 - 130 °C
 16.0 µm/m-°C
@Temperature 30.0 - 130 °C
High-expansive component
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 20.0 W/m-K
@Temperature 20.0 °C
Maximum Service Temperature, Air 550 °C
Minimum Service Temperature, Air -20.0 °C
 
Descriptive Properties
Linearity Range, °C-20 to 500
linearity Temperature Range, °C-20 to 550
Specific thermal curvature, /K0.0000094
Specific deflection, /K0.000005

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Precipitation Hardening Stainless

NSANDV130 / 19024

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.