MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chevron Phillips Synfluid® Dimer C12 Polyalphaolefin Reactive Olefinic Intermediate
Categories: Fluid

Material Notes: Synfluid® Dimer C12 is a reactive olefinic intermediate typically containing about 24 carbon atoms. Because Dimer remains a liquid at temperatures well below 0 ºC, it is useful in making derivatives whose flow properties are critical.

information provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.810 g/cc
@Temperature 15.6 °C
0.810 g/cc
@Temperature 60.0 °F
Density 0.808 g/cc0.0292 lb/in³
Viscosity Measure 858 cSt
@Temperature -40.0 °C
858 cSt
@Temperature -40.0 °F
Kinematic Viscosity
Kinematic Viscosity at 40°C (104°F) 7.7 cSt7.7 cSt
Kinematic Viscosity at 100°C (212°F) 2.3 cSt2.3 cSt
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.030<= 0.030
 
Thermal PropertiesMetricEnglishComments
Pour Point -47.2 °C-53.0 °F
Flash Point 183 °C362 °F
 
Descriptive Properties
AppearanceClear and bright
Color, Pt-Co0
Fire Point396°F
Odornone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCHEVP9924 / 242007

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.