TYRIL™ styrene-acrylonitrile (SAN) resins are designed to offer superior chemical resistance, strength, hardness and dimensional stability in a broad range of product applications. The key property of TYRIL 867 E is excellent balance of physical properties. TYRIL 867 E is specifically designed to provide good processability, good chemical and heat resistance and very good strength. The UV-stabilized version exhibits excellent weatherability, suitable in particular for extruded sheet and thermoforming applications. Applications: - Small appliances: transparent kitchen-robot parts
- Extruded sheet for shower cabinets, light-diffusers
- Houswares: food storage containers
- Sanitary accessories: soap dishes, toilet seats
Complies with:- Europe Food-Contact Compliance
- FDA, 21 CFR.181.32
Information provided by Trinseo. |