MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AGC SUNSPERA™ MB Silica Gel Catalyst Support
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Silica gels, as catalyst supports for manufacturing PE & PP, have important roles; more than carriers of active catalyst materials. Properties of silica gel significantly affect the polymerization process and the properties of finished polymer. SUNSPERA™, developed for catalyst supports, has precisely designed pore structure, spherical shapes, and size distribution. SUNSPERA™ offers improved morphology of finished polymer resins and productivity.

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 5.0 - 40 µm5.0 - 40 µm
Specific Surface Area 450 m²/g450 m²/g
 
Descriptive Properties
Pore diameter30 nm
Pore volume1.8 ml/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC SUNSPERA™ HH Silica Gel Catalyst Support
AGC SUNSPERA™ LB Silica Gel Catalyst Support
AGC SUNSPERA™ D-70-120A(LV) Silica Gel Catalyst Support
AGC SUNSPERA™ HB Silica Gel Catalyst Support
AGC SUNSPERA™ H-32 Silica Gel

PAGCX273 / 191382

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.