Description: Poly bd® R45 HTLO resin is a low molecular weight, liquid hydroxyl terminated polymer of butadiene. Poly bd® resins have primary, predominantly allylic hydroxy groups that exhibit high reactivity in chemical reactions for the preparation of derivatives. Product Highlights / Performance Properties: - Electrical insulative properties
- Miscibility with asphalt
- High solids loading
- Hydrolytically stable
- Good water resistance
- Low moisture permeability
- Resistance to aqueous acids and bases
- Low temperature flexibility
- Excellent adhesion to a variety of substrates
Suggested Applications: - Adhesives and sealants
- Coatings
- Electrical potting and encapsulation Polymer modification
- Polyurethanes
- Binders
Information provided by Cray Valley |