MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Regalite™ R7100 Hydrocarbon Resin
Categories: Other Engineering Material

Material Notes: Product Description: Regalite™ R7100 Hydrocarbon Resin is a partially hydrogenated water-white inert thermoplastic resin derived from petrochemical feedstocks. This resin is especially designed as a tackifier in hot melt adhesives based on SBS block copolymers, providing excellent color retention upon aging.

Application/Uses:

  • Automotive
  • Building and Construction
  • Hot Melt Adhesives
  • Pressure sensitive adhesives
  • Rubber and Plastic Modification
  • Solventborne Adhesives
  • Wax Modification

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/cc
Viscosity 120 cP
@Temperature 180 °C
Melt
 550 cP
@Temperature 160 °C
Melt
 3100 cP
@Temperature 140 °C
Melt
Molecular Weight 600 g/molMn
 900 g/molMw. Mw/Mn ratio = 1.5
 1400 g/molMz
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 49.0 °C
Ring & Ball Softening Point 102 °CASTM E28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 1.0ASTM D6166
 
Descriptive Properties
Cloud Point66°CMMAP
ColorHunterlab b, 5 cm path length

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5550 / 222744

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.