MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Kennametal Stellite Stellite® 98M2 with P/M Processing
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wear parts. Data provided by the manufacturer, Deloro Stellite, Inc.

Product of former Deloro Stellite Inc.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.45 g/ccP/M (98%)
 8.63 g/ccTheoretical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 58Hot hardness.
Tensile Strength, Ultimate 794 MPa
 656 MPa
@Temperature 760 °C
 690 MPa
@Temperature 649 °C
 725 MPa
@Temperature 538 °C
Elongation at Break 0.30 %in 25.4 mm
 0.30 %
@Temperature 538 °C
in 25.4 mm
 0.50 %
@Temperature 649 °C
in 25.4 mm
 0.50 %
@Temperature 760 °C
in 25.4 mm
 
Electrical PropertiesOriginal ValueComments
Magnetic Permeability <= 1.2
@Temperature 22.0 °C
116 Oersted
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.8 µm/m-°C
@Temperature 20.0 - 100 °C
 11.1 µm/m-°C
@Temperature 20.0 - 200 °C
 11.5 µm/m-°C
@Temperature 20.0 - 300 °C
 11.7 µm/m-°C
@Temperature 20.0 - 400 °C
 12.1 µm/m-°C
@Temperature 20.0 - 500 °C
 12.7 µm/m-°C
@Temperature 20.0 - 600 °C
 13.0 µm/m-°C
@Temperature 20.0 - 700 °C
 13.4 µm/m-°C
@Temperature 20.0 - 800 °C
 13.7 µm/m-°C
@Temperature 20.0 - 900 °C
 14.1 µm/m-°C
@Temperature 20.0 - 1000 °C
Melting Point 1224 - 1275 °C
Solidus 1224 °C
Liquidus 1275 °C
 
Component Elements PropertiesOriginal ValueComments
Boron, B 1.0 %
Carbon, C 2.0 %
Chromium, Cr 30 %
Cobalt, Co 31 %As remainder
Iron, Fe <= 5.0 %
Manganese, Mn <= 1.0 %
Molybdenum, Mo <= 0.80 %
Nickel, Ni 3.5 %
Other <= 2.0 %
Silicon, Si <= 1.0 %
Tungsten, W 18.5 %
Vanadium, V 4.2 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kennametal Stellite Stellite® 21
Kennametal Stellite Stellite® 25 Cobalt Chromium Cast Alloy
Kennametal Stellite Stellite® 3 PM cast
Kennametal Stellite Stellite® 3 PM with P/M Processing
Kennametal Stellite Stellite® 31 PM after P/M processing, aged 8 hours at 802°C air cooled

NS98MA / 18889

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.