MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® D1118 K (SBS) Diblock Copolymer
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D1118 K is a clear, diblock copolymer based on styrene and butadiene with a polystyrene content of 33%. It is supplied from North America in the physical form identified:
Kraton D1118 KT - supplied as a dusted porous pellet
Kraton D1118 KTM - supplied as a dusted powder

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton D1118 K is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings.

Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and Roofing

Note 1) The final dusting level is a combination of the talc from the original D1118 KT plus PGA-SD Alumina added during the milling process

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccASTM D4025
Volatiles <= 1.0 %KM 04
Viscosity 470 - 790 cP25% Toluene Solution at 25°C; BAM 922
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Ash 0.40 - 0.65 %KT, Talc; BAM 908
 4.0 - 6.0 %KIM, See Note 1); BAM 908
 
Chemical PropertiesOriginal ValueComments
Diblock Content 78 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 74
@Time 10.0 sec
Typical values on polymer compression molded at 350°F; ASTM D2240
Tensile Strength 1.72 MPaTypical properties of film cast from toluene solution; ASTM D412
Elongation at Break 600 %Measured on films cast from a solution in toluene; ASTM D412
300% Modulus 0.00120 GPa
@Strain 300 %
film cast from poluene solution; ASTM D412
 
Descriptive Properties
ContentNon-staining phenolic antioxidant0.15-0.4%, KM 08
 Polystyrene31-35%, KM 03
 Total Extractables<1.0%, KM 05
Styrene/Rubber Ratio33/67

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution K-Resin® KR03 Styrene Butadiene Copolymer (SBC)
INEOS Styrolution K-Resin® KR01 Styrene Butadiene Copolymer (SBC)
A. Schulman Diamond SBS 1031 Clear Styrene Butadiene Copolymer
Kraton® D1152 E (SBS) Liner Block Copolymer
Kraton® D1155 E (SBS) Liner Block Copolymer

PKRA9819 / 132718

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.