MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rogers Corporation Poron® Shock Seal™ 4790-79-20 Urethane Foam, Industrial Grade
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Thickness: 0.062"- 0.188"
Color: Black

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.320 g/cc0.0116 lb/in³ASTM D3574-95 Test A
Water Absorption 10 %
@Time 7200 sec
10 %
@Time 2.00 hour
Immersion; ASTM D570
Thickness 1570 - 4780 microns62.0 - 188 milRange of Thicknesses Available
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 0.689 MPa>= 100 psiASTM D3574-75 Test E
Elongation at Break >= 145 %>= 145 %ASTM D3574-75 Test E
Compressive Yield Strength 0.0276 - 0.110 MPa
@Strain 25 %
4.00 - 16.0 psi
@Strain 25 %
0.2"/min. strain rate
Tear Strength >= 1.80 kN/m>= 10.3 pliASTM D642-91 Die C
Compression Set  <= 5.0 %
@Temperature 23.0 °C
<= 5.0 %
@Temperature 73.4 °F
ASTM D3574-95 Test D
 <= 10 %
@Temperature 70.0 °C
<= 10 %
@Temperature 158 °F
ASTM D3574-95 Test D
 
Descriptive Properties
Flammability TestpassMVSS 302; 0.062 in.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Corporation Poron® 4790-79SP-15012 Urethane Shock Pad Foam
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft
Rogers Corporation Poron® ThinStik ShockSeal™ 79-09021 Self-Adhesive Urethane Foam
Rogers Corporation Poron® Shock Seal™ 4790-79-15 Urethane Foam, Industrial Grade
Rogers Corporation Poron® Shock Seal™ 4790-79-12 Urethane Foam, Industrial Grade

PROGA934 / 138374

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.