MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teknor Apex Monprene® OM-10150 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene OM-10150 is a thermoplastic elastomer designed for overmolding applications like grips and anti-skid parts for consumer products. Monprene OM-10150 is an opaque, UV resistant grade that exhibits excellent adhesion to nylon.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Good Mold Release; Good Moldability; Good Processability; High Flow; Light Stabilized; Low Density; Low Specific Gravity; Lubricated; Medium Hardness; Slip; Without Fillers

Uses: Appliances; Bonding; Cell Phones; Flexible Grips; Handles; Knobs; Overmolding; Power/Other Tools; Rubber Replacement; Sporting Goods; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ASTM D792
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 190 °C
35 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5353ASTM D2240
 50
@Time 5.00 sec
50
@Time 0.00139 hour
ASTM D2240
Tensile Strength at Break 2.43 MPa353 psi20 in/min, Across Flow; ASTM D412
 2.83 MPa410 psi20 in/min, Flow; ASTM D412
Tensile Stress at Strain  1.34 MPa
@Strain 100 %
195 psi
@Strain 100 %
20 in/min, Across Flow; ASTM D412
 1.63 MPa
@Strain 100 %
237 psi
@Strain 100 %
20 in/min, Flow; ASTM D412
 2.05 MPa
@Strain 300 %
297 psi
@Strain 300 %
20 in/min, Across Flow; ASTM D412
 2.76 MPa
@Strain 300 %
400 psi
@Strain 300 %
20 in/min, Flow; ASTM D412
Elongation at Break 340 %340 %20 in/min, Flow; ASTM D412
 350 %350 %20 in/min, Across Flow; ASTM D412
Tear Strength 14.5 kN/m83.0 pli20 in/min, Flow; ASTM D624
 16.3 kN/m93.0 pli20 in/min, Across Flow; ASTM D624
Compression Set 20 %
@Temperature 22.8 °C,
Time 79200 sec
20 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 204 - 232 °C400 - 450 °F
Middle Barrel Temperature 210 - 232 °C410 - 450 °F
Front Barrel Temperature 216 - 238 °C420 - 460 °F
Nozzle Temperature 221 - 243 °C430 - 470 °F
Melt Temperature 221 - 243 °C430 - 470 °F
Mold Temperature 23.9 - 60.0 °C75.0 - 140 °F
Drying Temperature 65.6 °C150 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 120 rpm50 - 120 rpm
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0885 / 237376

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.