MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Algoflon® F 5/S PTFE, Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Bronze Filled

Material Notes: Algoflon® F 5/S is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing powder. It is designed for compounds production and in particular it is recommended for use with high filler content. This material exhibits high bulk density, tensile strength and elongation at break. Black compounds based on Algoflon® F5/S show optimum isotropic behavior and therefore excellent longitudinal mechanical properties.

Main features of Algoflon® F 5/S are:

- High bulk density
- Very good mechanical properties
- Excellent blendability
- Very good electrical properties
- Isotropic properties

Applications: Additive; Blending

Features: Chemical Resistant

Processing
- Algoflon® F 5/S is used for preparing filled products based on PTFE resins. Prior to use, the powder needs to be conditioned above 19°C/66°F. In order to obtain fully homogeneous compounds, it is necessary to mix Algoflon® F 5/S and filler with high shear systems.
- Temperature must also be controlled (it should not rise above 40°C/104°F) during the mixing process to avoid agglomeration of PTFE and generation of white spots.
- Algoflon® F 5/S based compounds are processed using normal compression molding as similar to virgin fine cut PTFE.

Storage and Handling
- Algoflon® PTFE fine cut powders must be stored and handled carefully to achieve defect free molding. Before use the temperature of the powder must be conditioned above 19 °C / 66 °F (between 21-27 °C / 70–81 °F). Below this temperature, the powder is difficult to mold without cracks. Too high temperatures should also be avoided to prevent powder lumping and poor flow.
- Storage and handling facilities should be clean since even very small foreign particles can cause defects in finished products. Keep resin drums closed and clean. Good housekeeping and careful handling are essential.
- Each drum contains two bags liner made of polyethylene resin. The external bag liner is used only to protect the PTFE powders against external contamination. It is recommended to remove and isolate the external liner before handling and opening the internal layer which is in contact with the PTFE powders.

Safety and Toxicology
- Before using Algoflon® PTFE fine cut powders, consult the product Material Safety Data Sheet and follow all label directions and handling precautions.
- As with all PTFE materials, handling and processing should only be carried out in well ventilated areas. Vapor extractor units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contact, wash with soap and water. In case of eye contact, flush with water immediately and seek medical help.
- Do not smoke in areas contaminated with powder, vapor or fumes.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.16 g/ccASTM D792
Bulk Density 0.410 g/ccASTM D4894
Particle Size 15 µmAverage
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 44.0 MPaASTM D4894
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
ColorWhite
FormsPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4027 / 279827

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.