MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Alliance RN-42M Radially Oriented NdFeB Magnet
Categories: Metal; Electronic/Magnetic Alloy

Material Notes: The technology for producing rare earth ring magnets with radial magnetic fields has been around for decades, however the cost of manufacturing them come to a point where the magnets are an affordable replacement to traditional multi segmented arcs. There are three main manufacturing methods for producing bonded and sintered radial oriented rings: Anisotropic Pressure Molding, Hot Pressing & Backward Extrusion, and Radial Rotating Field Alignment. Each of these methods produces magnets with certain advantages and disadvantages over the others.

Information provided by Alliance LLC.

Key Words: Permanent Magnet
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density >= 7.40 g/cc>= 0.267 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 290.0 MPa42060 psi
Compressive Strength 780.00 MPa113130 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000150 ohm-cm
@Temperature 20.0 °C
0.000150 ohm-cm
@Temperature 68.0 °F
Magnetic Coercive Force, Hc 9700 - 11700 Oe9700 - 11700 Oe
 13000 - 15000 Oe13000 - 15000 OeIntrinsic
Magnetic Remanence, Br 12200 - 13000 Gauss12200 - 13000 Gauss
Magnetic Maximum Energy Product, BH 34 - 42 MGOe34 - 42 MGOe
Curie Temperature 310 °C590 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear -4.80 µm/m-°C-2.67 µin/in-°FPerpendicular to M
 3.40 µm/m-°C1.89 µin/in-°FParallel to M
Maximum Service Temperature, Air <= 100 °C<= 212 °FContinuous
 
Descriptive Properties
Reversible Temperature Coefficients-0.12Bd. %/°C
 -0.6Hd. %/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NALLIAN9928 / 268464

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.