MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical Lupoy 1302UV-08 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, UV Stabilized

Material Notes: Description: LUPOY PC 1302UV-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.

Main Characteristics: High viscosity and 0% UV light transmittance at wavelength below 400 nm

Applications: Lenses, Goggles, Sun Glasses and Appliances

CAS: 103598-77-2

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Water Absorption 0.15 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Moisture Absorption at Equilibrium 0.32 %
@Temperature 23.0 °C
50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cmASTM D955
Melt Flow 8.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 73ASTM D785
Hardness, Rockwell R 118ASTM D785
Tensile Strength, Ultimate 734 kg(f)/cm²ASTM D638
Tensile Strength, Yield 612 kg(f)/cm²50mm/min; ASTM D638
Elongation at Break 150 %ASTM D638
Elongation at Yield 6.0 %ASTM D638
Tensile Modulus 24600 kg(f)/cm²ASTM D638
Flexural Yield Strength 979 kg(f)/cm²ASTM D790
Flexural Modulus 24600 kg(f)/cm²ASTM D790
Izod Impact, Notched 92.53 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
0.25 mm notch; ASTM D256
Izod Impact, Unnotched NB
@Temperature 23.0 °C
ASTM D256
Dart Drop, Total Energy 89.0 J
@Thickness 3.20 mm
203m/min; ASTM D3763
Abrasion 45
@Load 1.00 kg
[%], CS-10 F wheel, 500 cycles; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+17 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 60 Hz
ASTM D150
Dielectric Strength 17.0 kV/mmASTM D149
Dissipation Factor 0.0010
@Frequency 60.0 Hz
ASTM D150
Arc Resistance 120 - 180 secASTM D495
Comparative Tracking Index 250 V
@Thickness 2.00 mm
IEC 112
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness >=1.60 mm
 30 - 60 sec
@Thickness >=2.50 mm
 30 - 60 sec
@Thickness >=3.00 mm
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 1.60 mm
 >= 120 arcs
@Thickness 2.50 mm
 >= 120 arcs
@Thickness 3.00 mm
High Voltage Arc-Tracking Rate, HVTR 25.4 - 50.0 mm/min
 
Thermal PropertiesOriginal ValueComments
CTE, linear 68.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
ASTM D696
Hot Ball Pressure Test >= 125 °CIEC 598-1
Deflection Temperature at 0.46 MPa (66 psi) 144 °C
@Thickness 4.00 mm
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 128 °C
@Thickness 4.00 mm
Unannealed; ASTM D648
 141 °C
@Thickness 4.00 mm
Annealed; ASTM D648
Vicat Softening Point 150 °C
@Load 5.10 kg
50°C/hr; ASTM D1525
Softening Point 150 - 200 °Cmelting point per MSDS
UL RTI, Electrical 80.0 °C
@Thickness >=0.500 mm
 120 °C
@Thickness >=1.60 mm
 120 °C
@Thickness >=2.50 mm
 120 °C
@Thickness >=3.00 mm
UL RTI, Mechanical with Impact 80.0 °C
@Thickness >=0.500 mm
 105 °C
@Thickness >=1.60 mm
 105 °C
@Thickness >=2.50 mm
 110 °C
@Thickness >=3.00 mm
UL RTI, Mechanical without Impact 80.0 °C
@Thickness >=0.500 mm
 120 °C
@Thickness >=1.60 mm
 120 °C
@Thickness >=2.50 mm
 120 °C
@Thickness >=3.00 mm
Flammability, UL94 V-2
@Thickness 0.500 mm
ASTM D635
 V-2
@Thickness 1.60 mm
ASTM D635
 V-2
@Thickness 2.50 mm
ASTM D635
 V-2
@Thickness 3.00 mm
ASTM D635
Flash Point >= 450 °C
Oxygen Index 26 %ASTM D2863
Glow Wire Test 850 °C
@Thickness 2.00 mm,
Time 5.00 sec
IEC 695-2-1
Ignition Temperature >= 450 °CAutoignition
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ASTM D542
Haze 0.70 - 1.5 %ASTM D1003
Transmission, Visible 89 %ASTM D1003
 
Descriptive Properties
Average Extent of BurningASTM D635

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical Lupoy 1201-08 Polycarbonate Resin
LG Chemical Lupoy 1302HP-22 Polycarbonate Resin
LG Chemical Lupoy 1302HP-07 Polycarbonate Resin
LG Chemical Lupoy 1302EP-30 Polycarbonate Resin
LG Chemical Lupoy 1302-10 Polycarbonate Resin

PLAY658 / 148668

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.