MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SisiB Silicones SiSiB® FS-0130 Hydrophilic fumed silica
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Composition: SiSiB® FS-0130 is a hydrophilic fumed silica with a specific surface area of 130 m2/g.

Introduction: Hydrophilic fumed silica is manufactured by hydrolysing volatile chlorosilanes in an oxyhydrogen flame. In chemical terms, the loose white powder consists of highly pure amorphous silicon dioxide. Hydrophilic silica is wetted by water and can be dispersed in water. Hydrophobic silica is produced by the chemical reaction of hydrophilic silica with reactive silanes, e.g. chlorosilanes or hexamethyldisilazane. It has water-repellent properties and is no longer dispersible in water.
All untreated fumed silicas are characterized by:

  • High purity
  • Aggregated structure
  • Submicron particle size
  • Low bulk density
  • Hydrophilic surface
CAS No: 112945-52-5 or 7631-86-9

EINECS No.: 231-545-4

Information provided by SiSiB Silicones - PCC Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0500 g/ccTamped
Particle Size 5.0 - 40 µm
pH 3.6 - 4.3in 4 % aqueous dispersion
Specific Surface Area 115 - 145 m²/gBET
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Component Elements PropertiesOriginal ValueComments
Loss on Ignition(%) <= 1.0 %
@Temperature 1000 °C,
Time 7200 sec
based on the substance dried at 105°C for 2 h
SiO2 >= 99.8 %based on the substance heated at 1000°C for 2 h
 
Descriptive Properties
Loss on drying<1.5%ex works (2h at 105 °C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSISIB001 / 318660

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.