MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lotte Advanced Materials PCN-2001 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Easy mold release; Available in transparent, translucent and opaque color

Applications: Multi purpose grade (electric/electronic housings, etc.)

Information provided by Lotte Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Maximum Moisture Content 0.02000.0200
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 63.7 MPa9250 psi50 mm/min; ASTM D638
Elongation at Break >= 100 %>= 100 %50 mm/min; ASTM D638
Flexural Strength 88.3 MPa12800 psi10 mm/min; ASTM D790
Flexural Modulus 2.35 GPa341 ksi10 mm/min; ASTM D790
Izod Impact, Notched 7.35 J/cm
@Thickness 3.17 mm
13.8 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 130 °C266 °FASTM D648
Flammability, UL94  V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
Shrinkage 0.00500 - 0.00700 %0.00500 - 0.00700 %ASTM D955
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FHopper
Rear Barrel Temperature 270 - 290 °C518 - 554 °F
Middle Barrel Temperature 260 - 280 °C500 - 536 °F
Front Barrel Temperature 250 - 270 °C482 - 518 °F
Nozzle Temperature 260 - 280 °C500 - 536 °F
Melt Temperature 270 - 290 °C518 - 554 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 120 °C
@Time 14400 sec
248 °F
@Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLOTT9291 / 325773

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.