MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Freudenberg Sealing Technologies 60 NR 11 Natural Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Elastomers made of pure natural rubber have extreme stretchability, ranging from 700 to 1000%. The elastomer is nearly non-compressible – it does not allow itself to be compressed – only displaced. Natural rubber is stable in acids, bases, water, alcohol and air, that is, in polar media. It has low media compatibility with nonpolar media such as petroleum-based oils, synthetic lubricants, brake fluids based on glycol, overheated moisture, and aromatic hydrocarbons (gasoline).

Information provided by Freudenberg Sealing Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/cc
@Temperature 23.0 °C
DIN EN ISO 1183-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 66
@Temperature 23.0 °C
DIN ISO 7619-1
Tensile Strength 21.1 MPaDIN 53504, S2
Elongation at Break 522 %
@Temperature 23.0 °C
DIN 53504, S2
100% Modulus 2.80 MPaDIN 53504, R1
Rebound 55 %DIN 53512
Compression Set 19 %
@Temperature 70.0 °C,
Time 86400 sec
DIN ISO 815
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °C
Minimum Service Temperature, Air -40.0 °C
 
Descriptive Properties
Colorblack
Gabo21.9
Loss Angle(°)8.3
Ozone resistance0DIN 53509

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFREU9045 / 293581

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.