MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Primex Plastics Prime Cor-X PP Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: Prime Cor-X PP is a Polypropylene that is extruded into a corrugated configuration that provides good stiffness. The surface can be corona treated so that it will accept inks for silk screening and other types of printing. The flute configuration can run parallel to the extrusion direction or they can be oscillating. A polyspunlaminate is also offered for this product.

Applications: Prime Cor-X PP is ideal for point of purchase displays, signs, mail totes, automotive dunnage and other types of containers. Furthermore, we also offer a polyspunlamination that will provide the prime surface with a low COF for protecting delicate products. Special formulas provide Conductive ( 104 -105 ohms/square) Anti-stat (109-1012ohms/square) and VCI (volatile corrosion inhibitor).

Information provided by Primex Plastics Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.906 g/cc0.906 g/ccASTM D792
Melt Flow 0.50 g/10 min0.50 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7575ASTM D785
Tensile Strength, Yield 27.6 MPa4000 psiASTM D638
Elongation at Break >= 500 %>= 500 %ASTM D638
Flexural Modulus 1.34 GPa195 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C190 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRIM013 / 278484

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.