Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,078-06-04-23 UL94 V-2, halogen and antimony free, medium impact polystyrene. This grade features enhanced thermal stability in the injection molding process and good mechanical properties. Applications: Examples of applications are TV back covers, printers and copiers. Unfilled. Suitable for Injection Molding. Supplied as pellets. Contains release agent. ISO data. Information provided by Enichem Versalis is the Eni subsidiary containing the plastics and rubber businesses. |