MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Akro-Plastic Akromid® B3 GK 30 natural PA 6 Conditioned, 30% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Bead Filled

Material Notes: Description: AKROMID B3 GK 30 natural is a 30% glass bead filled polyamide 6 with low warpage and high surface finish and light inherent color. Applications re housings and covers in the automotive, electro and furniture industry.

Features:

  • Good Surface Finish
  • Low Warpage
Uses:
  • Automotive Application
  • Electrical/Electronic Applications
  • Furniture
  • Housings

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Moisture Absorption 2.1 %
@Temperature 70.0 °C
2.1 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
Water Absorption at Saturation 6.5 %6.5 %ISO 62
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 90.0 MPa13100 psiH 358/30; ISO 2039-1
Tensile Strength at Break 38.0 MPa5510 psi5 [mm/min]; ISO 527-2
Elongation at Break 35 %35 %5 [mm/min]; ISO 527-2
Tensile Modulus 1.82 GPa264 ksi1 [mm/min]; ISO 527-2
Flexural Strength 55.0 MPa7980 psi2 [mm/min]; ISO 178
Flexural Modulus 1.57 GPa228 ksi2 [mm/min]; ISO 178
Charpy Impact Unnotched 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FDIN EN 11357-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKRO343 / 182930

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.