MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kingfa PC-S609 Toughened PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Impact Modified

Material Notes:
    Features:
  • Good mechanical properties
  • Super high impact strength
  • Good weather resistance
  • High gloss
  • Good processing properties
  • Stress cracking properties

    Applications:
  • OA and IT parts
  • Automobile accessories
  • Electrical and electronic parts
  • Switch and plug
  • Household appliance

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/cc
@Temperature 23.0 °C
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Temperature 23.0 °C
ASTM D955
Melt Flow 12 - 16 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 58.0 MPa50mm/min; ASTM D638
Elongation at Break >= 60 %50mm/min; ASTM D638
Flexural Strength 82.0 MPa2mm/min; ASTM D790
Flexural Modulus 2300 MPa2mm/min; ASTM D790
Izod Impact, Notched >= 450 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched NB
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+15 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 131 °C
@Thickness 6.40 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
@Thickness 6.40 mm
ASTM D648
Flammability, UL94 V-2
@Thickness 1.60 mm
 V-2
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 275 °C
Rear Barrel Temperature 240 - 270 °CStart Point: 240°C
Middle Barrel Temperature 240 - 260 °CStart Point: 235°C
Front Barrel Temperature 250 - 260 °CStart Point: 240°C
Melt Temperature 240 - 280 °CStart Point: 250°C
Mold Temperature 40.0 - 80.0 °CStart Point: 60°C
Drying Temperature 100 - 115 °C
@Time 10800 - 14400 sec
Pre-dry
Back Pressure 0.300 - 1.00 MPa
 
Descriptive Properties
Injection Speed60-90%
Weather Resistance (delta E)ASTM D4459; 200hr xenon lamp

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 1899 Polycarbonate, Impact Grade
Mitsubishi Xantar® G4F 23 UR Polycarbonate-20% Glass Reinforced
LG Chemical LUPOY SC1004L PC, High Impact
Kingfa JH820 Modified PC
Lehvoss LUVOCOM® 50/TF/15/BK Polycarbonate with PTFE

PKINGF087 / 104346

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.