MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Saint-Gobain Chemfab® 13 Tear Resistant PTFE-Coated Glass
Categories: Ceramic; Glass; Glass Fiber

Material Notes: Description: Chemfab® Tear Resistant Series is manufactured with specialized coating materials to improve tear and crease resistance. Uses for this series includes release sheets, belting and gaskets, and other applications where superior tear strength is required. All data based on a 0.013 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.0847 g/cc0.075306 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tear Strength Test 1212Lbs./In. for warp/longitudinal Propagation Tear Strength
 1515Lbs./In. Propagation Tear Strength in fill/transverse direction
Tear Strength 43.8 kN/m250 pliTensile Strength (Fill)
 61.4 kN/m350 pliTensile Strength (Warp)
 
Descriptive Properties
Weight (oz/yd^2)20.3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese VECTRA E135i LCP, 35% Glass Reinforced
Celanese VECTRA E130i LCP, 30% Glass Reinforced
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
Overview of materials for Acetal Homopolymer, PTFE-Filled
Hexcel® HexTow® AS4C 6K Standard Modulus Carbon Fiber (6000 Filaments)

CSTGQZ167 / 2296

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.