MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plenco 08133 Polyester BMC, Compression Molded  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: PLENCO 08133 is a renumber of PlasGlas 10313. PLENCO 08133 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its combination of high heat resistance, good electrical properties, flame resistance and strength, it can be used in such applications as iron skirts and other small appliance housings, coil bobbins, and electric motor components such as brush holders. It is available in either bulk or extruded form and is currently available in black. Other colors are available upon request. It is UL recognized under file E40654.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.85 g/ccASTM D792
Water Absorption 0.065 %ASTM D570
Linear Mold Shrinkage 0.0037 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 40ASTM D785
Tensile Strength, Ultimate 37.0 MPaASTM D638
Elongation at Break 0.52 %ASTM D638
Tensile Modulus 12.7 GPaASTM D638
Flexural Strength 99.0 MPaASTM D790
Flexural Modulus 11.6 GPaASTM D790
Compressive Strength 134 MPaASTM D695
Izod Impact, Notched 222 J/mASTM D256
Charpy Impact, Notched 2.35 J/cm²ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.40e+11 ohm-cmASTM D247
Dielectric Constant 19.1ASTM D150
Dielectric Strength 2.61 kV/mmShort Time; ASTM D149
 5.80 kV/mmStep by Step; ASTM D149
Dissipation Factor 0.40ASTM D150
Arc Resistance 180 secASTM D495
Comparative Tracking Index 600 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 218 °CHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 272 °CASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
Shrinkage 0.00 %72 hr, 120ºC; ASTM D1299

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyester Glass Filled BMC
A. Schulman BMC 1901 Mineral Filled Alkyd
Raschig Group RALUPOL® 2100 UP Polyester
Overview of materials for Silicone Rubber
Envalior Durethan® AKV 15 000000 Nylon 66, 15% Glass Fiber

PLEM55m2 / 50740

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.