MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Blue River Coatings CRC100-H
Categories: Polymer; Adhesive; Thermoset

Material Notes: BLUE RIVER COATINGS CRC100-H is a two-component inorganic corrosion resistant coating designed for Original Equipment Manufacturers (OEM) to protect metal substrates from corrosion and abrasion. If gouged or damaged, the coating will not experience creep and is repairable. The product is designed to coat surfaces that require a hard, abrasive, and chemical resistant coating that can withstand temperatures of 1,800°F. CRC100-H offers excellent durability and corrosion protection as well as being a low VOC and EPA compliant coating.

Environmental Advantages:BLUE RIVER COATINGS CRC100-H is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be dried and sent to a “Class B” landfill. Follow local and state regulations in the proper use and disposal of this product.

Characteristics:

  • Excellent hardness
  • Excellent adhesion to oxidized metal Excellent hardness
  • Excellent heat tolerance (1800°F+)
  • Excellent acid resistance
  • Good impact resistance and flexibility
  • Available in flat finish only
  • Non-photochemically reactive
  • Application by spraying or dipping
  • Solvent is used for clean-up
  • Air dry
  • Product life of 48 hours
  • Uses

  • Steel
  • Aluminum\
  • Information provided by Blue River Coatings

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity >= 1.00 g/cc>= 1.00 g/cc
    Density 1.21 g/cc0.0437 lb/in³
    Solids Content 47.5 %47.5 %by volume
     48 %48 %by weight
    Volatile Organic Compounds (VOC) Content 246 g/l246 g/l
     
    Mechanical PropertiesMetricEnglishComments
    Impact Test 18.1 J13.3 ft-lbForward and Reverse
     
    Thermal PropertiesMetricEnglishComments
    Flash Point 8.33 °C47.0 °FPart A
     65.6 °C150 °FPart B
     
    Processing PropertiesMetricEnglishComments
    Cure Time  240 min
    @Temperature 75.0 °C
    4.00 hour
    @Temperature 167 °F
    Recoat, at 50% humidity
     720 min
    @Temperature 75.0 °C
    12.0 hour
    @Temperature 167 °F
    Dust Free, at 50% humidity
     
    Descriptive Properties
    Evaporation rateSlower than ether
    Flexibility1/8" conical mandrel
    Pencil Hardness4H
    Salt SprayPassNon-oxidized steel panel, 2,000 hours with no blistering, creepage, cracking, peeling, or delamination.
     Pass;Oxidized steel panel, 1000 hours no blistering, creepage, cracking, peeling or delamination.
    Solvent Resistance20; double rubs with lacquer thinner, acetone, MEK, and xylene with saturated cloth
    Submersion Test>5 yearsliquid fertilizer (nitrogen) with no blistering, cracking, peeling or delamination.
     30 minutes30 minutes in Hydrochloric Acid (10%) with no blistering cracking peeling or delamination.
     30 minutesSulfuric Acid (10%) with no blistering, cracking, peeling or delamination.
    Theoretical Coverage762 ft2 at 1 mil

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    WBLUER13 / 74612

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.