MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Elmet Technologies Pure Molybdenum Sheet
Categories: Metal; Nonferrous Metal; Molybdenum Alloy; Refractory Metal; Pure Element

Material Notes: The chemical composition complies with ASTM requirements for powder lot analysis. Actual finished part chemical analysis and mechanical properties are not routinely evaluated per ASTM requirements. ASTM specifications and test methods are used as guidelines to control and monitor production processes to assure product quality. Applicable ASTM Material Standards: B386-91 (re-approved 1997) for plate/sheet/foil. This product meets the requirements of low copper and mercury-free materials.

Information provided by Elmet Technologies.

Vendors: Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 10.22 g/cc0.3692 lb/in³
a Lattice Constant 3.1399 Å3.1399 Å
Vapor Pressure  1.01058e-025 bar
@Temperature 787 °C
7.58e-023 torr
@Temperature 1450 °F
 1.97317e-020 bar
@Temperature 927 °C
1.00e-17 torr
@Temperature 1700 °F
 3.44e-15 bar
@Temperature 1227 °C
2.58e-12 torr
@Temperature 2241 °F
 1.05e-12 bar
@Temperature 1527 °C
7.88e-10 torr
@Temperature 2781 °F
 2.05e-7 bar
@Temperature 2127 °C
0.000154 torr
@Temperature 3861 °F
 0.0000240 bar
@Temperature 2727 °C
0.0180 torr
@Temperature 4941 °F
 0.00211 bar
@Temperature 3227 °C
1.58 torr
@Temperature 5841 °F
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 95.9495.94
Atomic Number 4242
Atomic Volume 9.419.41[cc/gm atom]
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 317 GPa46000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.00000552 ohm-cm
@Temperature 27.0 °C
0.00000552 ohm-cm
@Temperature 80.6 °F
 0.00000740 ohm-cm
@Temperature 100 °C
0.00000740 ohm-cm
@Temperature 212 °F
 0.00001315 ohm-cm
@Temperature 327 °C
0.00001315 ohm-cm
@Temperature 621 °F
 0.0000171 ohm-cm
@Temperature 500 °C
0.0000171 ohm-cm
@Temperature 932 °F
 0.0000222 ohm-cm
@Temperature 700 °C
0.0000222 ohm-cm
@Temperature 1290 °F
 0.00002951 ohm-cm
@Temperature 927 °C
0.00002951 ohm-cm
@Temperature 1700 °F
 0.00003814 ohm-cm
@Temperature 1227 °C
0.00003814 ohm-cm
@Temperature 2241 °F
 0.00004702 ohm-cm
@Temperature 1527 °C
0.00004702 ohm-cm
@Temperature 2781 °F
 0.00005306 ohm-cm
@Temperature 1727 °C
0.00005306 ohm-cm
@Temperature 3141 °F
 0.00005918 ohm-cm
@Temperature 1927 °C
0.00005918 ohm-cm
@Temperature 3501 °F
 0.00006537 ohm-cm
@Temperature 2127 °C
0.00006537 ohm-cm
@Temperature 3861 °F
 0.00007161 ohm-cm
@Temperature 2327 °C
0.00007161 ohm-cm
@Temperature 4221 °F
 0.0000779 ohm-cm
@Temperature 2527 °C
0.0000779 ohm-cm
@Temperature 4581 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  5.20 µm/m-°C
@Temperature 20.0 °C
2.89 µin/in-°F
@Temperature 68.0 °F
 5.80 µm/m-°C
@Temperature 2000 °C
3.22 µin/in-°F
@Temperature 3630 °F
 6.50 µm/m-°C
@Temperature 2500 °C
3.61 µin/in-°F
@Temperature 4530 °F
Specific Heat Capacity 0.270 J/g-°C0.0645 BTU/lb-°F
Thermal Conductivity  83.7 W/m-K
@Temperature 1500 °C
580 BTU-in/hr-ft²-°F
@Temperature 2730 °F
 105 W/m-K
@Temperature 1000 °C
725 BTU-in/hr-ft²-°F
@Temperature 1830 °F
 121 W/m-K
@Temperature 500 °C
841 BTU-in/hr-ft²-°F
@Temperature 932 °F
 138 W/m-K
@Temperature 100 °C
957 BTU-in/hr-ft²-°F
@Temperature 212 °F
 142 W/m-K
@Temperature 20.0 °C
986 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 2610 °C4730 °F
Boiling Point 4612 °C8334 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0025 %<= 0.0025 %
Cadmium, Cd <= 0.0015 %<= 0.0015 %
Calcium, Ca <= 0.0020 %<= 0.0020 %
Carbon, C <= 0.0050 %<= 0.0050 %
Chromium, Cr <= 0.0020 %<= 0.0020 %
Copper, Cu <= 0.0010 %<= 0.0010 %
Iron, Fe <= 0.0050 %<= 0.0050 %
Lead, Pb <= 0.0010 %<= 0.0010 %
Magnesium, Mg <= 0.0010 %<= 0.0010 %
Molybdenum, Mo >= 99.95 %>= 99.95 %
Nickel, Ni <= 0.0050 %<= 0.0050 %
Nitrogen, N <= 0.0020 %<= 0.0020 %
Other, each <= 0.0020 %<= 0.0020 %
Oxygen, O <= 0.0050 %<= 0.0050 %
Potassium, K <= 0.0030 %<= 0.0030 %
Silicon, Si <= 0.0025 %<= 0.0025 %
Sodium, Na <= 0.0020 %<= 0.0020 %
Tin, Sn <= 0.0020 %<= 0.0020 %
Tungsten, W <= 0.030 %<= 0.030 %
 
Descriptive Properties
Electron Work Function4.2 eV
Lattice StructureBody Centered Cubic
RoHS Compliance2002/95/EC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NELMET923 / 242044

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.