MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Durez® 33304 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Durez 33304 Phenolic Resin is a solvent-free, water-soluble resin. Durez 33304 resin provides superior strength, adhesion, and wetability for both organic and inorganic substrates. This unique water-soluble resin provides comparable or superior strength to solvent-based systems. When used in fiberglass or carbon composites, Durez 33304 provides excellent composite and interlaminary strength. In abrasive applications, Durez 33304 provides superior strength to inorganic grits and backing substrates. Designed for adhesion in both natural and synthetic substrates, Durez 33304 has excellent adhesion to fiberglass, carbon fiber, nylon, polyester, Kevlar, cotton and paper-based substrates. Durez 33304 eliminates the problem of conventional water systems in its ability to wet-out and coat synthetic substrates. This resin is equal to solvent-based systems in its ability to evenly coat synthetic substrates such as polyester, nylon and Kevlar.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 26 %DCT 4005A-1
pH 9.0DCT 4064A
Viscosity Measurement 1250
@Temperature 25.0 °C
DCT 4003F
 
Descriptive Properties
Water Tolerance, %350DCT 4012A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cotton Cloth Fiber
Solvay RHODAFAC® RS-610 Surfactant

PSUMIT287 / 194092

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.