MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

HP Alloys Alloy C-276, 20% Cold Worked
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.

Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes International.

Key Words: ASME SB-622, ASME SB-626 ASTM B-574, ASTM B-575, ASTM B-619; NACE MR-01-75, ASTM B-622, ASTM B-626, DIN 17744 No. 2.4602, TUV Werstoffblatt 479, UNS N06022, ASME SB-574, ASME SB-575, ASME SB-619, C276
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.90 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1021 MPa148100 psi
Tensile Strength, Yield 889 MPa129000 psi
Elongation at Break 26 %26 %
Modulus of Elasticity 205 GPa29700 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000130 ohm-cm0.000130 ohm-cm
Magnetic Permeability 1.00021.0002at 200 Oersted (15.9 kA/m)
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.7 µm/m-°C
@Temperature 20.0 - 100 °C
6.50 µin/in-°F
@Temperature 68.0 - 212 °F
 12.0 µm/m-°C
@Temperature 24.0 - 204 °C
6.67 µin/in-°F
@Temperature 75.2 - 399 °F
 12.8 µm/m-°C
@Temperature 23.9 - 316 °C
7.11 µin/in-°F
@Temperature 75.0 - 600 °F
 13.2 µm/m-°C
@Temperature 23.9 - 427 °C
7.33 µin/in-°F
@Temperature 75.0 - 800 °F
 13.4 µm/m-°C
@Temperature 24.0 - 538 °C
7.44 µin/in-°F
@Temperature 75.2 - 1000 °F
Specific Heat Capacity 0.427 J/g-°C0.102 BTU/lb-°F
Thermal Conductivity 10.5 W/m-K72.9 BTU-in/hr-ft²-°F
Melting Point 1325 - 1370 °C2417 - 2500 °F
Solidus 1325 °C2417 °F
Liquidus 1370 °C2500 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.010 %<= 0.010 %
Chromium, Cr 14.5 - 16.5 %14.5 - 16.5 %
Cobalt, Co <= 2.5 %<= 2.5 %
Iron, Fe 4.0 - 7.0 %4.0 - 7.0 %
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 15 - 17 %15 - 17 %
Nickel, Ni 57 %57 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si <= 0.080 %<= 0.080 %
Sulfur, S <= 0.010 %<= 0.010 %
Tungsten, W 3.0 - 4.5 %3.0 - 4.5 %
Vanadium, V <= 0.35 %<= 0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
HP Alloys Alloy C-276, 30% Cold Worked
Special Metals INCONEL® Alloy C-276
HP Alloys Alloy 718, 20% Cold Worked
Special Metals INCONEL® Alloy 686 Nickel Superalloy 30% Cold Worked (UNS N06686)
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 5% Cold Work

NPH271 / 18783

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.