MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Mylar® WC11/WC22 Polyester Film, 284 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Mylar® type WC11 films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectric and good handling characteristics.
  • Mylar® type WC11 is a single layer of Mylar® WC base corrugated in the length direction.
  • Mylar® type WC11G is a single layer of Mylar® WC base corrugated and also embossed with flat bands at 1/4" intervals in the transverse direction.
  • Mylar® type WC22 is a dual layer of Mylar® WC base corrugated in the length direction.
These modifications improve mechanical protection and serve as a heat barrier during extrusion coating of conductors.

Mylar® type WC11 films combine the tensile strength, dimensional stability, and dielectric strength needed for wire and cable applications.

Typical Applications: Mylar® Type WC11 films possess the characteristics required for wire and cable used in telecommunications and power transmission fields.

Approvals: UL 94 VTM-2 - for 142 - 300 gauge (0.036 - 0.076 mm)

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccTypical Mylar®; ASTM D1505
Thickness 2.84 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 125 %ASTM D882A
Film Elongation at Break, TD 100 %ASTM D882A
Film Tensile Strength at Break, MD 28000 psiASTM D882A
Film Tensile Strength at Break, TD 34000 psiASTM D882A
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 1937 V/mil1/4" electrode 500 V/sec 25°C in air; ASTM D149
Dielectric Breakdown 5500 V1/4" electrode 500 V/sec 25°C in air; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.17 J/g-°CTypical Mylar®
Melting Point 254 °CTypical Mylar® via DSC
Shrinkage, MD 1.5 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
Shrinkage, TD 1.0 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
 
Optical PropertiesOriginal ValueComments
Haze 18 %ASTM D1003
 
Descriptive Properties
Yield (nominal)6900 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDTZ9438 / 139755

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.