MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Zircar Refractory Composites RS-1200 Refractory Sheet
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: ZIRCAR Refractory Sheet Type RS-1200 is a high strength composite designed for use as thermo-mechanical and electrical insulation in applications with temperatures as high as 1300°C(2372°F). RS-1200 is a combination of strong reinforcing fibers tightly bound in an alumina ceramic matrix. RS-1200 is completely inorganic and contains no asbestos or RCF fibers. RS-1200 exhibits greater refractoriness and homogeneity than other reinforced alumina matrix composite products and can be readily machined to tight tolerances with conventional carbide tooling.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.16 g/cc0.0780 lb/in³
Loss On Ignition 1.0 - 2.0 %
@Temperature 982 °C
1.0 - 2.0 %
@Temperature 1800 °F
Porosity 31 %31 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 85 - 9085 - 90
Modulus of Rupture 0.0310 GPa4.50 ksiparallel to thickness
Compressive Yield Strength 55.0 MPa7980 psiat 2% compression parallel to thickness
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.20e+11 ohm-cm7.20e+11 ohm-cm
Surface Resistance 2.30e+11 ohm2.30e+11 ohm
Dielectric Strength 2.80 kV/mm71.0 kV/in
Dielectric Breakdown 7300 V7300 V1/8 in. thick
Arc Resistance >= 420 sec>= 420 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 µm/m-°C
@Temperature 20.0 - 400 °C
5.00 µin/in-°F
@Temperature 68.0 - 752 °F
Specific Heat Capacity 1.172 J/g-°C
@Temperature 600 °C
0.2801 BTU/lb-°F
@Temperature 1110 °F
Thermal Conductivity  0.620 W/m-K
@Temperature 200 °C
4.30 BTU-in/hr-ft²-°F
@Temperature 392 °F
parallel to thickness
 0.650 W/m-K
@Temperature 400 °C
4.51 BTU-in/hr-ft²-°F
@Temperature 752 °F
parallel to thickness
 0.660 W/m-K
@Temperature 600 °C
4.58 BTU-in/hr-ft²-°F
@Temperature 1110 °F
parallel to thickness
 0.680 W/m-K
@Temperature 1000 °C
4.72 BTU-in/hr-ft²-°F
@Temperature 1830 °F
parallel to thickness
Melting Point 1500 °C2730 °F
Maximum Service Temperature, Air 1300 °C2370 °F
Flammability Test 0.000.00Nil
Shrinkage  0.70 %
@Temperature 1100 °C,
Time 86400 sec
0.70 %
@Temperature 2010 °F,
Time 24.0 hour
perpendicular to thickness
 1.0 %
@Temperature 1300 °C,
Time 86400 sec
1.0 %
@Temperature 2370 °F,
Time 24.0 hour
perpendicular to thickness
 
Component Elements PropertiesMetricEnglishComments
Al2O3 82 %82 %
Other 6.0 %6.0 %
SiO2 12 %12 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AR-Glass Fiber, Generic
Crystex Composites Mykroy/Mycalex MM 411 Moldable Glass-Mica Composite
Crystex Composites Mykroy/Mycalex 555 Molding Grade Glass-bonded Mica Composite
Crystex Composites Mykroy/Mycalex MM 600 Machining Grade Glass-bonded Mica Composite
Crystex Composites Mykroy/Mycalex MM 800 Machining Grade Glass-bonded Mica Composite

CZRCI22 / 2885

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.