MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lucobit Lucocell® PE3700 Cellulose Asphalt Additive
Categories: Polymer; Thermoplastic; Cellulosic; Polyolefin

Material Notes: Lucocell® PE3700 granules – cellulose additives for SMA –Stone Mastic Asphalt or Split Mastic Asphalt, which is used as finish for all road types. Due to their 3D structure, cellulose fibers maintain a comparatively high viscosity of bitumen, thus preventing its seepage and formation of asphalt mix segregation at high temperatures during storage, transport and SMA placing. At the same time they enable creation of a thicker bitumen layer around each rock particle, thus preventing oxidation, moisture penetration and lifting or cracking of the aggregate.

Due to the pre-dispersion of cellulose fibers in the ethylene copolymer matrix of Lucocell® PE3700 the fibers release easily and safely for increased efficiency and improved production quality.

Information provided by Lucobit AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Apparent Bulk Density 0.370 g/cc
 
Descriptive Properties
Average Fiber Diameter, µm45
Average Fiber Length, µm1100
Ethylene Copolymer0.37

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUCO912 / 150978

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.