Hifax TYC 1087P 848 Black has a very high melt flow for easy and fast molding. It has excellent stiffness and cold temperature impact with very low CLTE. It is typically used for mold in color exterior applications. Availability: North America Application: Exterior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: High Stiffness; Low Temperature Impact Resistance Information provided by LyondellBasell. |