MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Polytek PlatSilĀ® FS-20 Liquid Silicone Rubbers
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: PlatSilĀ® FS-Series (Fast-Setting) Liquid Silicone Rubbers are two-component, room temperature curing mold rubbers. This series offers fast-setting formulations with long pour times relative to their cure speed. This allows for fast turn-around of molds and parts with sufficient time to mix and pour. PlatSil silicone rubbers are platinum-catalyzed, which, unlike tin-catalyzed systems, do not shrink on cure or deteriorate over time. Molds made from PlatSil rubbers offer good chemical resistance, making them a good choice when planning to cast polyesters, polyurethanes (plastic, foam, rubber), epoxies and more. PlatSil rubbers offer excellent release properties, making release agents unnecessary in many applications. Polytek offers additives to vary the viscosity and cure time of the liquid rubber, as well as hardness and color of the cured rubber.

Product Line Features:

  • Fast-setting formulas with long pour times
  • Low viscosity for excellent reproduction of details and easy degassing
  • Easy 1A:1B mix ratios by weight
  • Cure at room temperature or accelerate with heat
  • Easy release properties; save on release agents
  • High tear strength; fewer prematurely torn molds
  • Good chemical resistance for longer mold life
  • Low/zero shrinkage for better dimensional reproduction

Information provided by Polytek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/cc
Viscosity 3800 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 20
Hardness, Shore OO 66
Tensile Strength 467 psi
Elongation at Break 626 %
Tear Strength 52.8 pliDie T
 148.2 pliDie B
 
Processing PropertiesOriginal ValueComments
Cure Time 0.4167 hourDemold Time
 8.00 minPour Time
 24.0 hourTotal Cure
 
Descriptive Properties
Cured ColorMilky White
Mix Ratio By Weight1A:1B
Part A ColorMilky White
Part B ColorMilky White
Specific Volume24.9 in3/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPTK5012 / 251004

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.