MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Redwood Plastics REDCO™ OIL Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: A special formulation of liquid lubricant is encapsulated during manufacturing providing lubrication at the bearing surface. Redco™ Nylon Oil is offered for applications where maintenance lubrication is difficult or impossible. Redco™ Nylon Oil also limits moisture absorption, making Redco™ Nylon Oil an ideal bearing material for submerged or critical tolerance applications. This grade is also available in Redco™ Nylon Natural Oil for food and beverage applications and is U.S.A, F.D.A compliant.

Typical Applications: Bearings, bushings, bottling, canning, packing, processing, friction and wear applications in marine environments, gears, sprockets and power transmission components, etc.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³
Water Absorption 1.0 - 5.0 %1.0 - 5.0 %Equilibrium
 0.60 - 1.2 %
@Time 86400 sec
0.60 - 1.2 %
@Time 24.0 hour
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 68.9 MPa
@Time 86400 sec
10000 psi
@Time 24.0 hour
Elongation at Break 20 - 40 %20 - 40 %
Tensile Modulus 2.41 - 3.00 GPa350 - 435 ksi
Flexural Strength 86.2 - 89.6 MPa12500 - 13000 psi
Flexural Modulus 2.41 - 3.10 GPa350 - 450 ksi
Compressive Strength 96.5 - 103 MPa14000 - 15000 psi10% Deflection
Coefficient of Friction 0.17 - 0.190.17 - 0.19Dry vs.Steel
Limiting Pressure Velocity 0.140 MPa-m/sec4000 psi-ft/min
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 µm/m-°C30.6 µin/in-°F
Maximum Service Temperature, Air 200 - 250 °C392 - 482 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREDW034 / 296600

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.