MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M AC-370 Class B-2 Aerospace Sealant
Categories: Polymer; Thermoset; Polysulfide Sealant/Adhesive

Material Notes: 3M Aerospace Sealant AC-370 Class B are fast cure, low density polysulfide sealants suitable for fuel tank and fuselage applications. These two-component, manganese dioxide cured sealants are solvent free and have outstanding resistance to aviation gasoline and jet fuel, as well as resistance to chemicals and petroleum product common to the aircraft industry. 3M AC-370 Class B Sealants maintain flexibility and bond strength on most metal substrates like aluminum, titanium, stainless steel, steel, and many coatings under extremes of temperature, weathering and stress. The mixed compound is a thixotropic paste easily applied by extrusion, injection gun or spatula. They have excellent tooling properties.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density <= 1.30 g/cccured 14 days @ 50% RH
Volatiles 2.5 %
Brookfield Viscosity 900000 - 1.60e+6 cPRVF #7 sp @ 2 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50 - 55cured 14 days @ 50% RH
Tensile Strength at Break 1.25 MPa12 days @ 60°C + 60 hrs @ 71°C + 6 hrs @ 82°C in JRF I
 1.72 MPaStandard Cure
 1.72 MPaStandard heat cycle (AMS)
 1.82 MPa12 days @ 60°C + 60 hrs @ 71°C + 6 hrs @ 82°C in JRF I + 24 hrs air dry @ 49°C + standard heat cycle (AMS)
 1.91 MPa72 hrs at standard temperature in AMS 3021
 1.91 MPa72 hrs at standard temperature in AMS 3020
Elongation at Break 55 %Standard heat cycle (AMS)
 56 %12 days @ 60°C + 60 hrs @ 71°C + 6 hrs @ 82°C in JRF I + 24 hrs air dry @ 49°C + standard heat cycle (AMS)
 407 %12 days @ 60°C + 60 hrs @ 71°C + 6 hrs @ 82°C in JRF I
 412 %Standard Cure
 452 %72 hrs at standard temperature in AMS 3021
 452 %72 hrs at standard temperature in AMS 3020
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °Ccured 14 days @ 50% RH
 182 °CShort term, cured 14 days @ 50% RH
Minimum Service Temperature, Air -54.0 °Ccured 14 days @ 50% RH
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 - 10.0 hour
Tack-Free Time 7.00 - 8.00 hour
Shelf Life 9.00 Month
@Temperature <=26.7 °C
 
Descriptive Properties
AppearanceBrownAccelerator
 Dark Gray
 Off WhiteBase

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM35372 / 170119

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.