MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric  (discontinued **)
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3K

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 745 MPa
@Temperature -55.0 °C
Dry
 855 MPa
@Temperature 24.0 °C
Dry
 855 MPa
@Temperature 71.0 °C
Dry
Tensile Modulus 62.7 GPa
@Temperature 71.0 °C
Dry
 63.4 GPa
@Temperature 24.0 °C
Dry
 64.8 GPa
@Temperature -55.0 °C
Dry
Flexural Yield Strength 276 MPaLong Beam, dry
Compressive Yield Strength 400 MPa
@Temperature 71.0 °C
Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C)
 655 MPa
@Temperature 24.0 °C
Dry
Compressive Modulus 59.3 GPa
@Temperature 71.0 °C
Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C)
 64.1 GPa
@Temperature 24.0 °C
Dry
Bearing Yield Strength 848 MPa
@Temperature 24.0 °C
Dry
Shear Strength 26.2 MPa
@Temperature 71.0 °C
Short Beam, Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C)
 60.0 MPa
@Temperature 24.0 °C
Short Beam, Jet Fuel (30 ± 1 days of Jet A Fuel (ASTM D1655) at 75 ± 5°F (24 ± 3°C)
 61.0 MPa
@Temperature 24.0 °C
Short Beam, Dry
 61.4 MPa
@Temperature 24.0 °C
Short Beam, Skydrol (30 ± 1 days of Type 2 Skydrol Hydraulic Fluid at 140 ± 5°F (60 ± 3°C)
 
Descriptive Properties
Dry Resin Content (%)37-41Prepreg
Flow (%)8-20
Wet Resin Content (%)52Laminate

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay Thornel® P-75 Carbon Fiber/Epoxy Advanced Composite System
Solvay Thornel® P-55 Carbon Fiber/Epoxy Advanced Composite System
Solvay LTM® 26EL Epoxy with T300 Woven Carbon Fiber Laminate
Hexcel® HexPly® 8552 Epoxy Matrix, Carbon Fabric Form
Overview of materials for Epoxy/Carbon Fiber Composite

PHEXC142 / 98612

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.