Crosslinked silicone and acrylic adhesive with 2 mil polyester film release liner backing on the silicone side and moisture stable PE coated kraft (60#) on the acrylic side. Features: - Chemical resistant
- High Temperature resistant
- Good conformability
- High adhesion
- Solvent resistant
- Plasticizer migration resistant - acrylic side
- Bonds well to LSE substrates - silicone side
Applications: Overlap splicing and laminating various silicone surfaces such as silicone foam, rubber and gaskets to non-silicone coated substrates. Information provided by Dielectric Polymers. |