MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC NORYL™ Resin ZM3640 Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ ZM3640 resin is a mineral reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This grade contains non-brominated, non-chlorinated flame retardant and has a UL94 flame rating of V1 at 1.5mm. NORYL ZM3640 resin exhibits high heat resistance, low warpage, good dimensional stability and is an excellent candidate for printer chassis applications.

Features: Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Good Stiffness,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage,Good Moldability,Good Mold Release,Easy Molding,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Melt Flow 24 g/10 min
@Load 2.16 kg,
Temperature 300 °C
24 g/10 min
@Load 4.76 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psi5 mm/min; ASTM D638
Elongation at Break 4.0 %4.0 %5 mm/min; ASTM D638
Flexural Strength 102 MPa
@Thickness 6.40 mm
14800 psi
@Thickness 0.252 in
yield; ASTM D790
Flexural Modulus 4.62 GPa
@Thickness 6.40 mm
670 ksi
@Thickness 0.252 in
ASTM D790
Izod Impact Notched 35.0 J25.8 ft-lbASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 42.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 48.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
26.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 103 °C
@Thickness 6.40 mm
217 °F
@Thickness 0.252 in
unannealed; ASTM D648
UL RTI, Electrical 65.0 °C149 °FUL 746B
UL RTI, Mechanical with Impact 65.0 °C149 °FUL 746B
UL RTI, Mechanical without Impact 65.0 °C149 °FUL 746B
Flammability, UL94 V-1
@Thickness >=1.50 mm
V-1
@Thickness >=0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 255 - 280 °C491 - 536 °F
Zone 2 230 - 275 °C446 - 527 °F
Zone 3 245 - 280 °C473 - 536 °F
Melt Temperature 255 - 280 °C491 - 536 °FInjection Molding
Mold Temperature 65.0 - 90.0 °C149 - 194 °F
Drying Temperature 90.0 - 95.0 °C194 - 203 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Vent Depth 0.00380 - 0.00510 cm0.00150 - 0.00201 in
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82482 / 290429

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.