MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mocom (ALBIS) ALTECH® PA66 ECO 4015/120 MR15 IM Nylon 66, 15% Talcum Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Base Polymer: Polyamide 66

Filler/Additive System: 15% talcum

Special Features: Impact modified, heat ageing stabilization, easy release (demolding), injection molding grade

Market Segment: Automotive, various

Typical Application: Wheel trims, various

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ISO 1183
Maximum Moisture Content 0.150.15
Linear Mold Shrinkage, Flow 0.013 - 0.017 cm/cm
@Time 86400 sec
0.013 - 0.017 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.011 - 0.015 cm/cm
@Time 86400 sec
0.011 - 0.015 in/in
@Time 24.0 hour
ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 77.0 MPa11200 psiISO 527
Elongation at Break 18 %18 %ISO 527
Elongation at Yield 6.0 %6.0 %ISO 527
Tensile Modulus 3.30 GPa479 ksiISO 527
Flexural Strength 95.0 MPa13800 psiISO 178
Flexural Modulus 3.30 GPa479 ksiISO 178
Charpy Impact Unnotched 25.0 J/cm²119 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.850 J/cm²4.04 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C172 °FISO 75-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °FInjection molding
Mold Temperature 80.0 - 100 °C176 - 212 °FInjection molding
Drying Temperature 80.0 °C
@Time 7200 - 43200 sec
176 °F
@Time 2.00 - 12.0 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolyamide 66

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PALBIS8773 / 242832

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.